1
|
EXDO6930186743
|
WASPALOY HF UNL FORGE QUAL
|
CARPENTER TECHNOLOGY CORPORATION
|
HITACHI METALS MMC SUPERALLOY LTD
|
2022-04-07
|
South Korea
|
109002 Kgs
|
54 PKG
|
|
2
|
EXDO6930180111
|
BARS PROFILES OF NICKEL ALLOYS
|
CARPENTER TECHNOLOGY CORPORATION
|
HITACHI METALS MMC SUPERALLOY LTD
|
2021-02-17
|
Japan
|
3836 Kgs
|
3 CAS
|
|
3
|
EXDO6930176031
|
BARS PROFILES OF NICKEL ALLOYS
|
CARPENTER TECHNOLOGY CORPORATION
|
HITACHI METALS MMC SUPERALLOY LTD
|
2020-07-23
|
Japan
|
915 Kgs
|
1 CAS
|
|
4
|
MZENYOKNYC177438
|
NICKEL ALLOY SCRAP INCO 718
|
ELG UTICA ALLOYS(HERKIMER),INC.
|
HITACHI METALS MMC SUPERALLOY, LTD.
|
2017-10-04
|
Japan
|
14635 Kgs
|
68 BAG
|
|
5
|
MZENYOKNYC176563
|
NICKEL ALLOY SCRAP INCO 718
|
ELG UTICA ALLOYS(HERKIMER),INC.
|
HITACHI METALS MMC SUPERALLOY, LTD.
|
2017-08-10
|
Japan
|
21831 Kgs
|
64 BAG
|
|
6
|
MZENYOKNYC176003
|
NICKEL ALLOY SCRAP INCO 718
|
ELG UTICA ALLOYS(HERKIMER),INC.
|
HITACHI METALS MMC SUPERALLOY, LTD.
|
2017-07-05
|
Japan
|
41574 Kgs
|
190 PKG
|
|
7
|
NNRGNNRT7617588
|
COBALT ALLOY ROD . . . . . ., . . . .
|
POLYMET CORP
|
HITACHI METALS MMC SUPERALLOY, LTD.
|
2017-04-16
|
Japan
|
414 Kgs
|
2 CAS
|
|
8
|
VHFLTYOTN1519711
|
COBALT ALLOY (HS# 8105.90)
|
HIGH PERFORMANCE ALLOYS, INC.
|
HITACHI METALS MMC SUPERALLOY, LTD
|
2015-11-27
|
Japan
|
129 Kgs
|
1 CAS
|
|
9
|
VHFLTYOTN1519555
|
COBALT ALLOY (HS#8105.90)
|
WEARTECH INTERNATIONAL INC
|
HITACHI METALS MMC SUPERALLOY, LTD
|
2015-10-28
|
Japan
|
338 Kgs
|
1 CAS
|
|
10
|
VHFLTYOTN1519074
|
NO.6B BAR(COBALT ALLOY) , HS#8105.90
|
WEARTECH INTERNATIONAL INC
|
HITACHI METALS MMC SUPERALLOY, LTD
|
2015-07-15
|
Japan
|
174 Kgs
|
1 CAS
|